Hva er hovedmaterialene til API 5L rørledningsrør?

Hva er hovedmaterialene til API 5L standard rørledningsrør?

 

Hovedmaterialene til API 5L standard rørledningsrør er:

1, PSL1 grade: A / A210, B / L245, X42 / L290, X46 / L320, X52 / L360, X56 / L390, X60 / L415, X65 / L450, X70 / L485, X80 / L555

2, PSL2 -karakter: BN/L245N, X42N/L290N, X46N/L320N, X52N/L360N, X56N/L390N, X60N/L415N, X65Q/L450Q, X70Q/L48Q, X80Q/L450Q, X70Q/L485q, x80q/L450q, x70q/L485q, x80q/L450Q, x70q/L41q, x65q/L450Q, x60Q/L40Q, x65q/L45S X46Q/L320Q, X52Q/L360Q, X56Q/L390Q, X60Q/L415Q.

3,Acid line pipe material: BNS/L245NS, X42NS/L290NS, X46NS/L320NS, X52NS/L360NS, X56NS/L390NS, X60NS/L415NS, X65QS/L450QS, X70QS/L485SQ, X80QS/L555QS, X42QS/L290QS, X60Q/L415Q, X60Q/L415Q, X65QS/L450QS, X70QS/L485SQ, X80QS/L555QS, X42QS/L290QS, X42QS/L290QS, X60q/l415q/l290qs, x46qs/l320qs, x52qs/l360qs, x56qs/l390qs, x60qs/l415qs

4, acid / or service pipeline pipe material: BNO / L245NO, X42NO / L290NO, X46NO / L320NO, X52NO / L360NO, X56NO / L390NO, X60NO / L415NO, X65QO / L450QO, X70QO / L485QO, X80QO/L555QO, X42QO/L290QO, X46QO/L320QO, X52QO/L360QO, X56QO/L390QO, X60QO/L415QO